13 Chrome Mechanical Tube

Legacy Tubular offers high-grade 13 Chrome Mechanical Tubes designed for corrosion mitigation of CO₂ in oil and gas operations. These materials are suitable for sour service conditions, particularly in wells with CO₂ and small amounts of H₂S.

product details

GRADES

GRADES

  • L80 13Cr
  • 13Cr-95 (HP2-13CR95M)
  • Super 13Cr-110 (HP2-13CR110)

SIZES

  • Mechanical Tube Size Range: 3.425 – 12.75

 

Chemical Composition

 CMnMoCrNiCuTiPSSiVAl
Min0.1500.250–12.000––––––––
Max0.2201.000–14.0000.5000.250–0.0200.0101.000––

 

Mechanical Properties

Tensile Strength655 MPa min95,000 psi min
Yield Strength552 MPa min655 MPa max
 80,000 psi min95,000 psi max
Total Elongation Under Load0.500 %–
Hardness23 Max HRC241 Max HBW

 

Chemical Composition

 CMnMoCrNiCuTiPSSiVAl
Min––1.50011.500––––––––
Max0.0301.0002.50013.5006.000–0.5000.0200.0050.5000.500–

 

Chemical Composition

S13CR CMnMoCrNiCuTiPSSiVN
UNS S41425Min
Max
–
0.050
0.5
1.5
1.5
2
12.00
15.00
4.00
7.00
–
0.30
–
–
–
0.02
–
0.005
–
0.50
–
–
0.06
0.12
UNS S41426Min
Max
–
0.03
–
0.05
1.5
3
11.5
13.5
4.5
6.5
–
–
0.01
0.5
–
0.02
–
0.005
–
0.5
–
0.5
–
–
UNS S41427Min
Max
–
0.03
–
1
1.5
2.5
11.5
13.5
4.5
6
–
–
–
0.01
–
0.02
–
0.005
–
0.5
0.1
0.5
–
–

 

Mechanical Properties

Tensile Strength724 MPa min105,000 psi min
Yield Strength655 MPa min827 MPa max
 95,000 psi min120,000 psi max
Total Elongation Under Load20.000 %–
Hardness28 Max HRC–
 

Mechanical Properties

min Max
95ksi
UNS S41425
Tensile
Yield
Hardness
105
95
–
–
112
28
UNS S41426 Tensile
Yield
Hardness
105
95
–
–
105
27
UNS S41427 Tensile
Yield
Hardness
105
95
–
–
112
29

 

Chemical Composition

 CMnMoCrNiCuTiPSSiVAl
Min––1.50011.500––––––––
Max0.0301.0002.50013.5006.000–0.5000.0200.0050.5000.500–

Mechanical Properties

Tensile Strength862 MPa min125,000 psi min
Yield Strength758 MPa min965 MPa max
 110,000 psi min140,000 psi max
Total Elongation Under Load15.000 %–
Hardness32 Max HRC–
 

Chemical Composition

S13CR CMnMoCrNiCuTiPSSiVN
UNS S41425Min
Max
–
0.050
0.5
1.5
1.5
2
12.00
15.00
4.00
7.00
–
0.30
–
–
–
0.02
–
0.005
–
0.50
–
–
0.06
0.12
UNS S41426Min
Max
–
0.03
–
0.05
1.5
3
11.5
13.5
4.5
6.5
–
–
0.01
0.5
–
0.02
–
0.005
–
0.5
–
0.5
–
–
UNS S41427Min
Max
–
0.03
–
1
1.5
2.5
11.5
13.5
4.5
6
–
–
–
0.01
–
0.02
–
0.005
–
0.5
0.1
0.5
–
–
 

Mechanical Properties

min Max
110ksi
UNS S41425
Tensile
Yield
Hardness
125
110
–
–
130
32
UNS S41426 Tensile
Yield
Hardness
115
110
–
–
130
32
UNS S41427 Tensile
Yield
Hardness
125
110
–
–
130
32

legacy tubular

EXPLORE ALL PRODUCTS